This is the G2571A glaze recipe. It has proven reliable and functional over many years on a wide range of clay bodies in the Plainsman Clays studio. By itself, it is a great liner glaze. It does not cutlery mark or stain or craze and it great to use. And it accepts colorants very well.
Recipes |
G2571A - Cone 10 Silky Dolomite Matte Base Glaze
A cone 10R dolomite matte having a pleasant silky surface, it does not cutlery mark, stain or craze on common bodies |
---|---|
Articles |
How to Liner-Glaze a Mug
A step-by-step process to put a liner glaze in a mug that meets in a perfect line with the outside glaze at the rim. |
Articles |
G1947U/G2571A Cone 10/10R Base Matte/Glossy Glazes
These starting recipes use no frits and work in oxidation/reduction and are inexpensive to make. They can be used as bases for the whole range of typical cone 10 pottery glazes (celadon, tenmoku, oatmeal, white matte, brown crystal). |
Articles |
Concentrate on One Good Glaze
It is better to understand and have control of one good base glaze than be at the mercy of dozens of imported recipes that do not work. There is a lot more to being a good glaze than fired appearance. |