Fired to cone 10 oxidation. Although feldspar is a key melter in high and medium temperature glazes, by itself it does not melt as much as one might expect in this GLFL test. The Montana materials on the right are not commercially available, they were being evaluated for viability.
Articles |
A Low Cost Tester of Glaze Melt Fluidity
This device to measure glaze melt fluidity helps you better understand your glazes and materials and solve all sorts of problems. |
---|---|
Materials | G-200 Feldspar |
Materials | Feldspar |
Tests | Glaze Melt Flow - Runway Test |
Glossary |
Melt Fluidity
Ceramic glazes melt and flow according to their chemistry and mineralogy. Observing and measuring the nature and amount of flow is important in understanding them. |
Glossary |
Feldspar Glazes
Feldspar is a natural mineral that, by itself, is the most similar to a high temperature stoneware glaze. Thus it is common to see alot of it in glaze recipes. Actually, too much. |