Floating Blue is a popular cone 6 glaze recipe used by the pottery community. Gerstley Borate is a material commonly used in recipes as a melter. The recipe produces a variegated surface but is difficult to replicate since its fragile mechanism makes it susceptible to variations in thickness, firing schedule, clay body and material supplies.
Materials | Boraq |
---|---|
Materials | Gerstley Borate |
Media |
Subsitute Gerstley Borate in Floating Blue Using Desktop Insight
Use Desktop Insight to explore ways of calculating substitutes for Gerstley Borate in the popular Floating Blue cone 6 glaze recipe while maintaining or improving the other raw and fired properties of the glaze. |
Recipes |
P3998 - Boraq 1 Recipe
Gerstley Borate substitute |