I weighed the bucket of glaze and then put about a third of it on a clean plaster surface to dewater. Then I put that back in the bucket and weighed it again. It was 400 grams lighter so I added 400 grams of Laguna Gum Solution. That changed it to a drip-drip-drip dipping glaze but it now dries much harder and I can do thick brushwork on it without worrying about it lifting off.
Materials | CMC Gum |
---|---|
Glossary |
Base-Coat Dipping Glaze
These are ceramic glazes intended for dipping but which contain a gum to enable them to adhere to the body better and tolerate over-layers without danger of flaking or cracking. |