Glaze is GA6-B Alberta Slip rutile blue base. Fired at cone 6. The "Mother Nature's porcelain". from which this piece is made, has 6% Mason 6600 black stain. This glaze is an amber transparent and on the black porcelain produces a blacker deeper color than a typical transparent would.
Recipes |
GA6-B - Alberta Slip Cone 6 Amber Base 2
An amber-colored glaze that produces a clean, micro-bubble-free transparent glass. Works well on brown and red burning stonewares. |
---|