Made in southern Alberta around around 1970. They were extruded and then hand assembled. These are on display in the salt glaze kiln next to the Plainsman factory.
Glossary |
Salt firing
Salt firing is a process where unglazed ware is fired to high temperatures and salt is introduced to produce a vapor that glazes the ware. |
---|