Monthly Tech-Tip | No tracking! No ads! |
Description: Lead Bisilicate frit, Loodbisilicaat Fritte
Oxide | Analysis | Formula | |
---|---|---|---|
PbO | 64.72% | 1.00 | |
SiO2 | 33.81% | 1.94 | |
Al2O3 | 1.48% | 0.05 | |
Oxide Weight | 344.90 | ||
Formula Weight | 344.90 |
Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
---|---|
Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
By Tony Hansen Follow me on |
Buy me a coffee and we can talk