Glasurfritten 35.055

Alternate Names: 35 055,35-055

Description: Bleimonosilikat-Fritte

Oxide Analysis Formula
PbO 78.80% 1.00
SiO2 21.20% 1.00
Oxide Weight 283.25
Formula Weight 283.25

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 90 x 10-7
Frit Softening Point 455C
Frit Melting Range (C) 900-1080C