Alternate Names: Ferro Feldspar #10
Description: Legacy feldspar
Oxide | Analysis | Formula | |
---|---|---|---|
K2O | 9.84% | 0.71 | |
Na2O | 2.59% | 0.29 | |
Al2O3 | 14.64% | 0.98 | |
SiO2 | 68.83% | 7.83 | |
LOI | 4.10% | n/a | |
Oxide Weight | 655.80 | ||
Formula Weight | 683.84 |
Typecodes |
Feldspar
The most common source of fluxes for high and medium temperature glazes and bodies. |
---|