Oxide Analysis Formula
SiO2 49.80% 2.53
Al2O3 33.40% 1.00
Fe2O3 1.20% 0.02
TiO2 0.48% 0.02
CaO 0.60% 0.03
MgO 0.40% 0.03
K2O 0.50% 0.02
Na2O 0.23% 0.01
LOI 12.59%n/a
Oxide Weight 264.50
Formula Weight 302.59