Bentolite L-2

Oxide Analysis Formula
CaO 1.67% 0.24
K2O 0.06% 0.01
MgO 3.65% 0.73
Na2O 0.20% 0.03
TiO2 0.28% 0.03
Al2O3 15.49% 1.22
SiO2 71.99% 9.64
Fe2O3 0.72% 0.04
LOI5.93%
Oxide Weight 757.32
Formula Weight 805.06

Related Information

Links

Materials Bentolite L
Materials Bentolite H
Typecodes Clay Other
Clays that are not kaolins, ball clays or bentonites. For example, stoneware clays are mixtures of all of the above plus quartz, feldspar, mica and other minerals. There are also many clays that have high plasticity like bentonite but are much different mineralogically.

By Tony Hansen


Tell Us How to Improve This Page

Or ask a question and we will alter this page to better answer it.

Email Address

Name

Subject

Message


CAPTCHA

Leave the following empty



https://digitalfire.com, All Rights Reserved
Privacy Policy