Notes
Old Number: 6
Use this to lighten stain colors (use 6768 to lighten cobalt blues, 6067 to lighten pinks).
Related Information
White stain. Does it work?
This is G2934Y matte glaze base with opacifiers added. It has been applied to a dark-burning body to demonstrate the comparative degrees of opacity. The stain is Mason 6700 white. While it does not opacify nearly as well as tin or zircon, it does produce a smoother surface.
Links
Materials |
Stain
|
Typecodes |
Colorant
Metallic based materials that impart fired color to glazes and bodies.
|