Materials Definition Table                 Name: AUST2.MDT
                                 Oxide Property: EXPAN
                              Material Property: COST/KG
------------------------------------------------------------

Num OXIDE/MATERIAL         WEIGHT    PROP  Oxides
-------------------------------------------------
  0 BaO                    153.40  12.900  BaO-1.00
  1 CaO                     56.10  14.800  CaO-1.00
  2 PbO                    223.20   8.300  PbO-1.00
  3 Li2O                    29.80   8.800  Li2O-1.00
  4 MgO                     40.30   2.600  MgO-1.00
  5 K2O                     94.20  33.100  K2O-1.00
  6 Na2O                    62.00  38.700  Na2O-1.00
  7 ZnO                     81.40   9.400  ZnO-1.00
  8 Fe2O3                  160.00  12.500  Fe2O3-1.00
  9 MnO                     71.00   9.000  MnO-1.00
 10 TiO2                    79.70   1.400  TiO2-1.00
 11 P2O5                   142.00          P2O5-1.00
 12 ZrO2                   123.00   9.900  ZrO2-1.00
 13 B2O3                    69.60   3.100  B2O3-1.00
 14 Al2O3                  102.00   6.300  Al2O3-1.00
 15 SiO2                    60.00   3.500  SiO2-1.00

Num OXIDE/MATERIAL         WEIGHT    PROP  Oxides
-------------------------------------------------
 16 BALL CLAY C            623.27   1.250  CaO- .06, MgO- .15, K2O- .12,
                                           Na2O- .04, Fe2O3- .05, TiO2- .12, Al2O3-1.00,
                                           SiO2-7.46
 17 BALL CLAY R            465.61   1.250  CaO- .02, MgO- .08, K2O- .11,
                                           Na2O- .04, Fe2O3- .03, TiO2- .09, Al2O3-1.00,
                                           SiO2-5.08
 18 BALL CLAY FX           374.50   1.250  CaO- .02, MgO- .09, K2O- .10,
                                           Na2O- .06, Fe2O3- .02, TiO2- .07, Al2O3-1.00,
                                           SiO2-3.60
 19 BALL CLAY H            497.03   1.250  CaO- .04, MgO- .12, K2O- .13,
                                           Na2O- .06, Fe2O3- .06, TiO2- .07, Al2O3-1.00,
                                           SiO2-5.44
 20 BALL BM                376.63          CaO- .01, MgO- .02, K2O- .01,
                                           Na2O- .01, Fe2O3- .02, TiO2- .17, Al2O3-1.00,
                                           SiO2-3.38
 21 BALL F                 414.20          CaO- .01, MgO- .08, K2O- .14,
                                           Na2O- .03, Fe2O3- .02, TiO2- .07, Al2O3-1.00,
                                           SiO2-4.21
 22 K37G                   276.37          CaO- .01, MgO- .01, K2O- .01,
                                           Na2O- .00, Fe2O3- .02, Al2O3-1.00, SiO2-2.24
 23 K38                    284.59          CaO- .01, MgO- .01, K2O- .00,
                                           Na2O- .00, Fe2O3- .02, Al2O3-1.00, SiO2-2.36
 24 BBR                    337.77          CaO- .00, MgO- .04, K2O- .02,
                                           Na2O- .02, Fe2O3- .01, TiO2- .04, Al2O3-1.00,
                                           SiO2-3.12
 25 BB4                    323.15          CaO- .01, MgO- .03, K2O- .02,
                                           Fe2O3- .01, TiO2- .05, Al2O3-1.00, SiO2-2.86
 26 BB8                    384.69          CaO- .01, MgO- .06, K2O- .02,
                                           Na2O- .01, Fe2O3- .05, TiO2- .05, Al2O3-1.00,
                                           SiO2-3.69
 27 BB12                   379.69          CaO- .00, MgO- .02, K2O- .02,
                                           Na2O- .01, Fe2O3- .01, TiO2- .05, Al2O3-1.00,
                                           SiO2-3.78
Num OXIDE/MATERIAL         WEIGHT    PROP  Oxides
-------------------------------------------------
 28 ALBANY SLIP            697.09   1.750  CaO- .72, MgO- .47, K2O- .24,
                                           Na2O- .09, Fe2O3- .23, TiO2- .04, Al2O3-1.00,
                                           SiO2-6.71
 29 ALBERTA SLIP           331.84   1.040  BaO- .00, CaO- .37, MgO- .27,
                                           K2O- .12, Na2O- .11, Fe2O3- .10, TiO2- .02,
                                           Al2O3- .47, SiO2-3.58
 30 ALUMINA CALCINED       102.00   2.000  Al2O3-1.00
 31 ALUMINA HYDRATE        156.00   1.240  Al2O3-1.00
 32 ANHYDROUS BORAX        201.20          Na2O-1.00, B2O3-2.00
 33 PITTONG P.L            269.70          CaO- .00, MgO- .00, K2O- .00,
                                           Na2O- .00, Fe2O3- .01, TiO2- .03, Al2O3-1.00,
                                           SiO2-2.10
 34 GLASS CULLET           205.97          CaO- .37, MgO- .17, K2O- .00,
                                           Na2O- .45, Fe2O3- .00, Al2O3- .02, SiO2-2.45
 35 FERRO FRIT 3110        260.76   4.550  CaO- .29, K2O- .06, Na2O- .64,
                                           B2O3- .10, Al2O3- .09, SiO2-3.03
 36 K10                    441.58          CaO- .03, MgO- .08, K2O- .10,
                                           Na2O- .06, Fe2O3- .04, TiO2- .08, Al2O3-1.00,
                                           SiO2-4.68
 37 WINGEN GROG            228.54          CaO- .01, MgO- .02, K2O- .00,
                                           Na2O- .00, Fe2O3- .03, Al2O3-1.00, SiO2-1.98
 38 OAKLANDS KAOLIN        283.04          CaO- .01, MgO- .02, K2O- .08,
                                           Na2O- .01, Fe2O3- .02, TiO2- .04, Al2O3-1.00,
                                           SiO2-2.23
 39 BALL CLAY              321.40    .350  CaO- .01, MgO- .02, K2O- .03,
                                           Na2O- .02, Fe2O3- .02, TiO2- .06, Al2O3-1.00,
                                           SiO2-2.78
 40 BARIUM CARBONATE       197.40   2.000  BaO-1.00
 41 BARIUM SULPHATE        233.13   1.470  BaO-1.00
 42 ECKAGLAS               272.47   1.400  K2O- .01, Na2O- .00, Fe2O3- .01,
                                           Al2O3-1.00, SiO2-2.16
 43 ECKALITE 1             265.00   1.600  Fe2O3- .01, TiO2- .02, Al2O3-1.00,
                                           SiO2-2.06
 44 ECKALITE 2             273.12   1.500  Fe2O3- .01, TiO2- .03, Al2O3-1.00,
                                           SiO2-2.16
 45 BALL BW                390.18          CaO- .01, MgO- .12, K2O- .08,
                                           Na2O- .01, Fe2O3- .04, TiO2- .06, Al2O3-1.00,
                                           SiO2-3.73
 46 BENTONITE              489.48   1.500  CaO- .04, MgO- .28, K2O- .15,
                                           Fe2O3- .11, TiO2- .01, Al2O3-1.00, SiO2-5.28
 47 BONE ASH               310.30   7.500  CaO-3.00, P2O5-1.00
 48 BORAX                  381.50   3.000  Na2O-1.00, B2O3-2.00
 49 BORIC ACID             123.62   2.230  B2O3-1.00
 50 HOME RULE 1            289.33          CaO- .01, MgO- .01, K2O- .00,
                                           Na2O- .00, Fe2O3- .03, TiO2- .05, Al2O3-1.00,
                                           SiO2-2.35
 51 CALCINED KAOLIN        222.00    .820  Al2O3-1.00, SiO2-2.00
 52 CALCIUM BORATE         205.51   1.100  CaO-1.00, B2O3-1.50
 53 CALCIUM CARBONATE      100.00    .120  CaO-1.00
 54 CALCIUM FELDSPAR       518.10    .400  CaO-1.00, Al2O3-1.00, SiO2-6.00
 55 CALCIUM PHOSPHATE      310.30   3.190  CaO-3.00, P2O5-1.00
 56 ECKALITE 120           272.80          K2O- .01, Na2O- .00, Fe2O3- .02,
                                           Al2O3-1.00, SiO2-2.16
 57 POT FELDSPAR PREMIU    566.67   1.900  K2O- .72, Na2O- .27, Fe2O3- .01,
                                           Al2O3-1.00, SiO2-6.23
 58 POT FELDSPAR STAND     566.67   1.500  CaO- .03, MgO- .01, K2O- .62,
                                           Na2O- .33, Fe2O3- .01, Al2O3-1.00, SiO2-6.33
Num OXIDE/MATERIAL         WEIGHT    PROP  Oxides
-------------------------------------------------
 59 COLEMANITE             205.50  12.980  CaO-1.00, B2O3-1.50
 60 CORNISH STONE          725.43   3.800  CaO- .23, MgO- .03, K2O- .33,
                                           Na2O- .39, Fe2O3- .01, TiO2- .01, Al2O3-1.16,
                                           SiO2-8.92
 61 CRYOLITE               210.53   8.500  Na2O-1.00, Al2O3- .33
 62 CUSTER FELDSPAR        617.10    .190  CaO- .03, K2O- .66, Na2O- .30,
                                           Fe2O3- .01, Al2O3-1.04, SiO2-7.10
 63 SILICA                 100.00   1.150  SiO2-1.67
 64 DOLOMITE               184.00   1.450  CaO-1.00, MgO-1.00
 65 ENGLISH KAOLIN         272.88    .950  CaO- .00, MgO- .02, K2O- .05,
                                           Na2O- .00, Fe2O3- .01, TiO2- .00, Al2O3-1.00,
                                           SiO2-2.15
 66 EPK KAOLIN             270.35    .420  CaO- .01, MgO- .01, K2O- .01,
                                           Fe2O3- .01, TiO2- .01, P2O5- .00, Al2O3-1.00,
                                           SiO2-2.10
 67 EUREKA FELDSPAR        638.20    .390  K2O- .64, Na2O- .36, Fe2O3- .00,
                                           Al2O3-1.07, SiO2-7.42
 68 FERRO FRIT 3124        277.93   5.900  CaO- .70, K2O- .02, Na2O- .28,
                                           B2O3- .55, Al2O3- .27, SiO2-2.56
 69 FERRO FRIT 3134        190.64   4.950  CaO- .68, Na2O- .32, B2O3- .63,
                                           SiO2-1.48
 70 FERRO FRIT 3195        337.36   2.340  CaO- .67, Na2O- .33, B2O3-1.11,
                                           Al2O3- .41, SiO2-2.67
 71 FERRO FRIT 3211        133.57   3.000  CaO-1.00, B2O3-1.11
 72 FERRO FRIT 3269        352.58   3.140  CaO- .01, K2O- .31, Na2O- .64,
                                           ZnO- .04, B2O3- .78, Al2O3- .46, SiO2-2.97
 73 FERRO FRIT 3278        270.44   3.000  CaO- .33, Na2O- .67, Al2O3- .57,
                                           SiO2-2.53
 74 FERRO FRIT 3300        207.93   3.000  BaO- .08, CaO- .33, PbO- .21,
                                           MgO- .02, K2O- .07, Na2O- .02, ZnO- .27,
                                           Al2O3- .19, SiO2-1.34
 75 FERRO FRIT 3304        382.45   2.490  PbO- .93, Na2O- .07, B2O3- .22,
                                           SiO2-2.58
 76 FERRO FRIT 3327        284.33   2.800  PbO-1.00, SiO2-1.02
 77 FERRO FRIT 3419        271.14   2.500  PbO- .72, Na2O- .28, B2O3- .57,
                                           SiO2- .89
 78 FERRO FRIT 3467        343.28   2.290  CaO- .49, PbO- .26, MgO- .05,
                                           K2O- .06, Na2O- .13, B2O3- .22, Al2O3- .31,
                                           SiO2-3.23
 79 FERRO FRIT 3481        292.95   2.470  CaO- .52, PbO- .30, K2O- .04,
                                           Na2O- .15, B2O3- .26, Al2O3- .20, SiO2-2.43
 80 FERRO FRIT 3602        341.81   2.370  PbO-1.00, Al2O3- .08, SiO2-1.83
 81 FLINT                   60.00    .190  SiO2-1.00
 82 FLUORSPAR               78.00    .870  CaO-1.00
 83 G200 FELDSPAR          550.59    .540  CaO- .13, K2O- .56, Na2O- .31,
                                           Fe2O3- .00, Al2O3-1.05, SiO2-6.06
 84 GEORGIA KAOLIN         263.16    .240  CaO- .00, MgO- .01, K2O- .01,
                                           Na2O- .01, Fe2O3- .01, TiO2- .04, Al2O3-1.00,
                                           SiO2-1.96
 85 GERSTLEY BORATE        133.20   7.500  CaO- .40, Na2O- .20, B2O3-1.00
 86 GOLDART                357.58    .340  CaO- .01, MgO- .02, K2O- .04,
                                           Na2O- .01, Fe2O3- .03, TiO2- .09, Al2O3-1.00,
                                           SiO2-3.42
 87 GROLLEG KAOLIN         274.19    .950  CaO- .00, MgO- .02, K2O- .06,
                                           Fe2O3- .01, Al2O3-1.00, SiO2-2.18
 88 HALLAM FIRE CLAY       286.35    .340  MgO- .01, K2O- .00, Na2O- .00,
                                           Fe2O3- .03, TiO2- .05, Al2O3-1.00, SiO2-2.29
Num OXIDE/MATERIAL         WEIGHT    PROP  Oxides
-------------------------------------------------
 89 HOMMEL FRIT 13         226.58   5.500  PbO- .70, Na2O- .30, B2O3- .39,
                                           SiO2- .41
 90 HOMMEL FRIT 22         385.67   4.900  CaO- .47, PbO- .53, B2O3- .98,
                                           SiO2-2.88
 91 HOMMEL FRIT 240        271.04   5.057  PbO- .72, Na2O- .28, B2O3- .56,
                                           SiO2- .90
 92 HOMMEL FRIT 266        245.79   4.500  CaO- .68, Na2O- .32, B2O3-1.10,
                                           Al2O3- .32, SiO2-1.31
 93 HOMMEL FRIT 267        301.77   4.500  CaO- .56, K2O- .13, Na2O- .31,
                                           B2O3-1.24, Al2O3- .29, SiO2-2.05
 94 HOMMEL FRIT 285        315.26   4.500  K2O- .10, Na2O- .90, B2O3- .94,
                                           Al2O3- .21, SiO2-2.72
 95 IRON OXIDE RED         160.00   2.600  Fe2O3-1.00
 96 STAWELL KAOLIN         457.60          MgO- .02, K2O- .07, Na2O- .01,
                                           Fe2O3- .03, TiO2- .01, Al2O3-1.00, SiO2-5.11
 97 JORDAN FIRECLAY        505.49    .490  CaO- .02, MgO- .06, K2O- .11,
                                           Na2O- .02, Fe2O3- .05, TiO2- .08, Al2O3-1.00,
                                           SiO2-5.66
 98 K&T S-2 BALL CLAY      421.02    .450  CaO- .02, MgO- .04, K2O- .06,
                                           Fe2O3- .03, TiO2- .07, Al2O3-1.00, SiO2-4.32
 99 K200 FELDSPAR          550.34    .450  CaO- .04, K2O- .60, Na2O- .34,
                                           Al2O3-1.00, SiO2-6.12
100 KAOLIN                 258.14   1.250  Al2O3-1.00, SiO2-2.00
101 KAOPAQUE KAOLIN        258.14    .500  Al2O3-1.00, SiO2-2.00
102 KINGMAN FELDSPAR       570.99    .450  CaO- .01, K2O- .73, Na2O- .26,
                                           Fe2O3- .00, Al2O3-1.05, SiO2-6.29
103 KONA A-3 FELDSPAR      658.79    .450  CaO- .05, K2O- .52, Na2O- .43,
                                           Fe2O3- .00, Al2O3-1.05, SiO2-7.85
104 KONA F-4 FELDSPAR      520.62    .450  CaO- .16, K2O- .27, Na2O- .58,
                                           Fe2O3- .00, Al2O3-1.00, SiO2-5.79
105 KY SPECIAL BALL CLA    355.83    .500  CaO- .03, MgO- .04, K2O- .03,
                                           Na2O- .01, Fe2O3- .02, TiO2- .07, Al2O3-1.00,
                                           SiO2-2.99
106 KYANITE                162.00          Al2O3-1.00, SiO2-1.00
107 LEAD CARBONATE         258.00   3.650  PbO-1.00
108 LEPIDOLITE             385.37   5.150  Li2O- .54, K2O- .39, Na2O- .07,
                                           Fe2O3- .00, Al2O3- .99, SiO2-3.72
109 LITHARGE               223.20          PbO-1.00
110 LITHIUM CARBONATE       73.40  20.500  Li2O-1.00
111 M&D BALL CLAY          373.21    .500  CaO- .03, MgO- .05, K2O- .02,
                                           Fe2O3- .05, TiO2- .06, Al2O3-1.00, SiO2-3.57
112 MAGNESIUM CARBONATE     84.31   4.600  MgO-1.00
113 MANGANESE CARBONATE    115.07   8.600  MnO-1.00
114 MANGANESE DIOXIDE       87.01   1.650  MnO-1.00
115 NEPHELINE SYENITE      446.40   1.850  CaO- .06, MgO- .01, K2O- .22,
                                           Na2O- .71, Al2O3-1.04, SiO2-4.53
116 NP BLEND BALL CLAY    1768.11    .260  CaO- .09, MgO- .18, K2O- .18,
                                           Na2O- .07, Fe2O3- .13, TiO2- .35, Al2O3-5.11,
                                           SiO2-   16.03
117 OM#4 BALL CLAY         356.64    .350  MgO- .04, K2O- .04, Fe2O3- .02,
                                           TiO2- .08, Al2O3-1.00, SiO2-3.30
118 OXFORD FELDSPAR        686.06    .450  CaO- .05, K2O- .59, Na2O- .36,
                                           Fe2O3- .00, Al2O3-1.17, SiO2-8.07
119 PBX FIRECLAY           264.80    .400  CaO- .02, MgO- .02, Fe2O3- .03,
                                           TiO2- .05, Al2O3-1.00, SiO2-2.49
120 PEARL ASH              165.26   2.050  K2O-1.00
121 PEARL ASH CALCINED     138.12          K2O-1.00
Num OXIDE/MATERIAL         WEIGHT    PROP  Oxides
-------------------------------------------------
122 PEMCO FRIT 316         363.90   4.509  PbO-1.00, Al2O3- .25, SiO2-1.92
123 PEMCO FRIT 349         312.60   4.900  CaO- .58, PbO- .24, K2O- .09,
                                           Na2O- .09, B2O3- .36, Al2O3- .19, SiO2-2.80
124 PEMCO FRIT 54          190.73   5.000  CaO- .68, Na2O- .32, B2O3- .64,
                                           SiO2-1.47
125 PEMCO FRIT 67          310.47   5.000  CaO- .69, K2O- .12, Na2O- .19,
                                           B2O3-1.16, Al2O3- .37, SiO2-2.17
126 PEMCO FRIT 83          341.96   4.900  PbO- .72, Na2O- .28, B2O3- .26,
                                           SiO2-2.43
127 PEMCO FRIT 926         225.99   5.000  CaO- .68, K2O- .01, Na2O- .31,
                                           B2O3- .61, Al2O3- .11, SiO2-1.90
128 PETALITE               662.33  10.800  Li2O- .96, K2O- .02, Na2O- .03,
                                           Al2O3-1.14, SiO2-8.50
129 PIONEER KAOLIN         258.14    .240  Al2O3-1.00, SiO2-2.00
130 PLASTIC VITROX        1158.12    .300  CaO- .05, MgO- .06, K2O- .84,
                                           Na2O- .05, Fe2O3- .01, Al2O3-1.69,
                                           SiO2-   14.57
131 POTASH FELDSPAR        556.20   1.900  K2O-1.00, Al2O3-1.00, SiO2-6.00
132 PYROPHILITE           2555.96    .730  CaO- .05, K2O- .38, Na2O- .49,
                                           Fe2O3- .08, Al2O3-5.01, SiO2-   31.31
133 RED LEAD               228.00          PbO-1.00
134 REDART                 631.65    .320  CaO- .03, MgO- .26, K2O- .29,
                                           Na2O- .04, Fe2O3- .29, TiO2- .09, P2O5- .01,
                                           Al2O3-1.00, SiO2-7.11
135 SAGGER XX BALL CLAY    349.70    .500  CaO- .03, MgO- .03, K2O- .03,
                                           Na2O- .02, Fe2O3- .02, TiO2- .07, Al2O3-1.00,
                                           SiO2-3.30
136 SLEDGE BALL CLAY       419.29    .570  CaO- .03, MgO- .04, K2O- .02,
                                           Fe2O3- .02, TiO2- .09, Al2O3-1.00, SiO2-4.39
137 SNOBRITE KAOLIN        256.73    .650  CaO- .01, Fe2O3- .01, TiO2- .02,
                                           Al2O3-1.00, SiO2-1.92
138 SODA ASH               105.98   2.100  Na2O-1.00
139 SODA FELDSPAR          524.00   1.500  Na2O-1.00, Al2O3-1.00, SiO2-6.00
140 SPODUMENE              400.03   2.900  CaO- .01, Li2O- .91, MgO- .01,
                                           K2O- .03, Na2O- .03, Fe2O3- .01, Al2O3-1.11,
                                           SiO2-4.18
141 SPRUCE PINE #4 SPAR    551.42    .450  CaO- .15, K2O- .29, Na2O- .55,
                                           Fe2O3- .00, Al2O3-1.03, SiO2-6.25
142 TALC                   126.23   1.350  MgO-1.00, SiO2-1.33
143 TENNESSEE #5 BALL      360.42    .570  CaO- .01, MgO- .03, K2O- .06,
                                           Na2O- .03, Fe2O3- .02, TiO2- .06, Al2O3-1.00,
                                           SiO2-3.29
144 TILE #6 KAOLIN         258.14    .280  Al2O3-1.00, SiO2-2.00
145 TITANIUM DIOXIDE        79.70   7.000  TiO2-1.00
146 VELVACAST KAOLIN       262.14    .660  CaO- .01, MgO- .01, Fe2O3- .01,
                                           TiO2- .04, Al2O3-1.00, SiO2-1.98
147 VOLCANIC ASH           577.00   2.220  CaO- .83, MgO- .10, K2O- .02,
                                           Na2O- .01, Fe2O3- .04, Al2O3- .12, SiO2-7.05
148 WHITING                100.00   1.250  CaO-1.00
149 WOLLASTONITE           116.10   3.500  CaO-1.00, SiO2-1.00
150 ZINC OXIDE              81.40   5.750  ZnO-1.00
151 CMC GUM                         8.290  
152 ZIRCONIUM SILICATE     183.00   5.200  ZrO2- .54, SiO2- .55
153 FERRO FRIT 4113        351.00   4.950  CaO- .60, K2O- .13, Na2O- .27,
                                           B2O3- .64, Al2O3- .35, SiO2-3.47
154 RAILTON LIMESTONE       62.86          CaO-1.00, Fe2O3- .00, Al2O3- .01,
                                           SiO2- .09
Num OXIDE/MATERIAL         WEIGHT    PROP  Oxides
-------------------------------------------------
155 ALBURY SLIP            275.22          CaO- .34, MgO- .33, K2O- .09,
                                           Na2O- .07, Fe2O3- .13, MnO- .00, TiO2- .03,
                                           P2O5- .00, Al2O3- .37, SiO2-2.80
156 BURNIE BASALT          172.13          CaO- .24, MgO- .46, K2O- .02,
                                           Na2O- .08, Fe2O3- .19, MnO- .00, TiO2- .04,
                                           P2O5- .00, Al2O3- .23, SiO2-1.25
157 STANLEY BASALT         184.89          CaO- .32, MgO- .35, K2O- .03,
                                           Na2O- .10, Fe2O3- .20, MnO- .00, TiO2- .04,
                                           P2O5- .01, Al2O3- .26, SiO2-1.33
158 COOEE DOLERITE         241.87          CaO- .37, MgO- .29, K2O- .06,
                                           Na2O- .10, Fe2O3- .18, MnO- .01, TiO2- .04,
                                           P2O5- .01, Al2O3- .38, SiO2-2.10
159 SPILITE                222.19          CaO- .37, MgO- .24, K2O- .01,
                                           Na2O- .13, Fe2O3- .24, MnO- .00, TiO2- .02,
                                           Al2O3- .36, SiO2-1.75
160 KMP4064                326.30   7.100  PbO- .95, Na2O- .05, Al2O3- .06,
                                           SiO2-1.74
161 KMP4101                323.70   6.000  CaO- .13, K2O- .19, Na2O- .69,
                                           B2O3- .62, Al2O3- .27, SiO2-2.81
162 KMP4108                229.10   4.950  CaO- .68, Na2O- .32, B2O3- .64,
                                           Al2O3- .07, SiO2-1.99
163 KMP4110                261.10   4.550  CaO- .29, K2O- .07, Na2O- .64,
                                           B2O3- .10, Al2O3- .11, SiO2-3.01
164 KMP4113                351.30   4.950  CaO- .60, K2O- .13, Na2O- .27,
                                           B2O3- .64, Al2O3- .35, SiO2-3.47
165 KMP4124                268.30   5.900  CaO- .68, K2O- .04, Na2O- .29,
                                           B2O3- .56, Al2O3- .16, SiO2-2.57
166 KMP4125                323.80          CaO- .14, K2O- .09, Na2O- .78,
                                           B2O3- .64, Al2O3- .25, SiO2-3.00
167 KMP4171                248.60   5.850  CaO- .49, Na2O- .51, B2O3- .77,
                                           SiO2-2.26
168 KMP4193                311.10   5.850  BaO- .10, CaO- .51, K2O- .09,
                                           Na2O- .19, ZnO- .10, B2O3- .62, Al2O3- .20,
                                           SiO2-2.89
169 KMP4300                272.10          CaO- .42, K2O- .09, Na2O- .19,
                                           MnO- .30, B2O3- .44, Al2O3- .25, SiO2-2.51
170 AVAIL                                  
171 AVAIL                                  
172 AVAIL                                  
173 AVAIL                                  
174 AVAIL                                  
175 AVAIL                                  
176 AVAIL                                  
177 AVAIL                                  
178 AVAIL                                  
179 AVAIL                                  
180 AVAIL                                  
181 AVAIL                                  
182 AVAIL                                  
183 AVAIL                                  
184 AVAIL                                  
185 AVAIL                                  
186 AVAIL                                  
187 AVAIL                                  
188 AVAIL                                  
189 AVAIL                                  
190 AVAIL                                  
Num OXIDE/MATERIAL         WEIGHT    PROP  Oxides
-------------------------------------------------
191 AVAIL                                  
192 AVAIL                                  
193 AVAIL                                  
194 AVAIL                                  
195 AVAIL                                  
196 AVAIL                                  
197 AVAIL                                  
198 AVAIL                                  
199 AVAIL                                  
200 AVAIL                                  

ESC to finish..




















