  • (Recipes) GR6-F - Ravenscrag Cone 6 High Alumina Matte

    Plainsman Cone 6 Ravenscrag Slip based glaze. It can be found among others at http://ravenscrag.com.

    2003-12-18 - This is a high alumina matte glaze and is a favorite. It is not temperature sensitive and produces good results at cone 5, 6 and 7 (medium blue surfac...

  • (Recipes) GR10-B - Ravenscrag Cone 10R Gloss Base

    Cone 10 Reduction glaze made using 90% Ravenscrag Slip.

    2005-02-22 - 100% Ravenscrag slip fires to a silky matte at cone 10R so you need to melt it a little more to get a good gloss. This version produces excellent r...

  • (Recipes) GR6-D - Ravenscrag Cone 6 Glossy Black

    Plainsman Cone 6 Ravenscrag Slip based glaze. It can be found among others at http://ravenscrag.com.

    2005-02-21 - Every potter wants a good reliable glossy black glaze that has a minimum of toxic metals and fires to an even color without pinholes and blisters. Rav...

  • (Recipes) GR6-C - Ravenscrag Cone 6 White Glossy

    Plainsman Cone 6 Ravenscrag Slip based white glossy glaze. It can be found among others at http://ravenscrag.com.

    2005-02-21 - A white base glaze with all the advantages of Ravenscrag Slip base GR6-A. It is not drab-looking like a porcelain toilet, but is vibrant and interesti...

  • (Recipes) GR6-A - Ravenscrag Cone 6 Clear Glossy Base

    This Plainsman Cone 6 Ravenscrag Slip base is just the pure material with 20% added frit to make it melt to a glossy natural clear.

    2003-07-21 - This is the base cone 6 Ravenscrag recipe, it fires as a transparent glossy. It has an addition of the most common North American borate frit, enough ...

  • (Recipes) GR6-B - Ravenscrag Cone 6 Variegated Light Glossy Blue

    Plainsman Cone 6 Ravenscrag Slip based glaze. It can be found among others at http://ravenscrag.com.

    0000-00-00 - This produces a variegated light medium blue glaze that breaks greenish over edges. This glaze is very consistent and has very good working properties...

  • (Recipes) GR6-E - Ravenscrag Cone 6 Raspberry Glossy

    A chrome-tin burgundy glaze using the Ravenscrag cone 6 base recipe.

    2005-02-21 - Chrome-tin (either from the raw materials or a stain) pink and red glazes can be difficult to achieve and keep consistent at cone 6. In ceramics, red ...

  • (Recipes) g2851H - Ravenscrag Cone 6 High Calcium Matte Blue

    Plainsman Cone 6 Ravenscrag Slip based glaze. It can be found among others at http://ravenscrag.com.

    2003-12-18 - This glaze is temperature sensitive. It requires a slow cool down to allow crystals to grow. If the kiln cools too quickly you will get a glossy gla...

  • (Recipes) G2853B - Cone 04 Clear Ravenscrag School Glaze

    A Ravenscrag Slip base made by simply mixing it 50:50 with a frit

    2004-01-07 - What is Needed: -Plainsman Buffstone (lowfire buff burning body) (for a class with 20 to 30 children, for two projects for each student, 2 to 3 b...

  • (Recipes) GR6-H - Ravenscrag Cone 6 Oatmeal Matte

    Plainsman Cone 6 Ravenscrag Slip glaze. See more at ravenscrag.com.

    2003-07-21 - Note: For use as a straight glaze We are recommending GA6-F Alberta Slip oatmeal glaze instead, it looks better and has a better melt. Alberta ...

  • (Recipes) GR10-A - Pure Ravenscrag Slip

    Ravenscrag all by itself makes a great cone 10 reduction semi-gloss glaze. It also has great working properties.

    2003-12-19 - Ravenscrag Slip is a revolutionary glaze material for stoneware. At cone 10R it can be used pure and produces a functional semi-gloss surface. The pos...