FLS - Flux Source

Materials that source Na2O, K2O, Li2O, CaO, MgO and other fluxes but are not feldspars or frits. Remember that materials can be flux sources but also perform many other roles. For example, talc is a flux in high temperature glazes, but a matting agent in low temperatures ones. It can also be a flux, a filler and an expansion increaser in bodies.

Out Bound Links

  • (Glossary) Flux

    On the theoretical glaze chemistry level, a flux is an oxide that lowers the melting or softening temperature of a mix of materials. Fluxes are interactors (they often melt poorly on their own but react strongly with high melting materials where Al2O3/SiO2 predominate). There are less than ten commo...

In Bound Links