Clays that are not kaolins, ball clays or bentonites. For example, stoneware clays are mixtures of all of the above plus quartz, feldspar, mica and other minerals. There are also many clays that have high plasticity like bentonite but are much different mineralogically.

Out Bound Links

  • (Glossary) Earthenware

    A clay fired at low temperatures (cone 010-02) where it does not develop maturity (vitrify). The term earthenware almost alway refers to red burning terra cotta ware (although it is a somewhat more general term referring to a wider range of colors and more primitive forming and firing techniques). E...