CGS - Crystalline Glaze Recipe Fara Shimbo

These are from Fara's Crystal Glazes book II.

In Bound Links

  • (Recipes) F5-3NO-E1 - Fa's Blue Heaven Fara Shimbo Crystalline

    Nickel teal crystals on a transparent amber ground

    2004-05-14 - This is so far the best base from which to obtain true nickel teal crystals (caused by nickel zinc silicate) on an amber ground (caused by nickel spin...

  • (Recipes) GBCG1 - Frit 3110 Generic Base Crystalline Glaze

    From Fara Shimbo Crystal Glaze book 2

    2008-03-20 - You can change the ratio of these ingredients to suit your individual needs and tastes, within certain parameters. The more frit you use (relative to ...

  • (Recipes) GBCG2 - Frit GCC106 Generic Base Crystalline Glaze

    From Fara Shimbo Crystal Glazes Book 2

    2008-03-20 - You can change the ratio of these ingredients to suit your individual needs and tastes, within certain parameters. The more frit you use (relative t...

  • (Recipes) GC - GC106 Base Fara Shimbo Crystalline Glaze

    Cone 9-10 for brilliant colors

    2004-05-14 - This is the most basic crystalline glaze recipe I know for use with this frit. It requires a slightly higher fire than bases made with the Ferro 3110...

  • (Recipes) TF - Tin Foil II Fara Shimbo Crystalline Glaze

    Low Titanium Cone 6-9 Glaze

    2004-05-14 - Purpose: To alter the shape of the crystals from broad "geranium" petals to narrow "dandelion" or "aster" petals by using tin. Tin Foil 2 is an ex...

  • (Recipes) GR - GRANITE Fara Shimbo Crystalline Glaze

    Zinc Silicate and Rutile Crystal Producing Glaze

    2004-05-12 - This glaze produces a surface coated with small crystals of rutile which grow both around and through the zinc silicate crystals. Surface is fairly s...

  • (Recipes) WM - Wollast-O-Matte Fara Shimbo Crystalline Glaze

    Matte textured crystalline glaze

    2004-05-14 - This is essentially a raw glaze which gives small crystals on a very tactile surface. It accepts most colorants easily (with the exception of nickel ...

  • (Recipes) VS - Vesuvius Fara Shimbo Crystalline Glaze

    Titanium-Free Crystalline Glaze

    2004-05-13 - Matures at cone 9. Completely transparent ground and easily grown crystals very white when no other colorants are used. Surface is relatively hard a...

  • (Recipes) AO - Fa's All-Opaque Base Fara Shimbo Crystalline

    Entirely opaque surface (crystals and ground)

    2004-05-13 - An excellent "starter glaze" for new crystallieri.

  • (Recipes) B1 - Bory 1 Fara Shimbo Crystalline Glaze

    High Boron, Opaque Cone 6-10 glaze

    2004-05-14 - Purpose: To obtain greater firing range and more "flowery" crystals by the addition of extra boron and calcium. Tony Hansen gave me the idea to try...

  • (Recipes) CE - Celestite Fara Shimbo Crystalline Glaze

    High Lithium, Low Titanium Cone 7-10 Glaze

    2004-05-12 - Purpose: To create a glaze which would give strong, dark, true turquoises from copper through copper's interaction with lithium. I noticed that in ...

  • (Recipes) ZZ1 - Zu-Zu Cone 8-9 Fara Shimbo Crystalline Glaze

    Lower fire version of a popular crystalline glaze

    2004-05-14 - This glaze utilizes the Glass Coatings and Concepts' (formerly General Color's) GF 106 Frit. This is a substitute for the popular Pemco 286 frit whic...