BSQ - Bisque Firing

Out Bound Links

  • (Glossary) Bisque, bisquit firing

    Generally, bisque firing refers to the practice of prefiring ware without glaze to make it impervious to water, resistant to damage during handling and absorbent for glazing. The porosity of the bisque (generally more than 15%) makes it an ideal medium to absorb water from the glaze suspension and h...