BIO - Biocide

These are added to glazes and bodies to prevent the growth of organics. Often classified as Bactericides or Fungicides.

Mold that has grown on pugged clay in a bag.

Amazing mold (actually sprouting leaves) that has grown on pugged clay after 10 months of storage where there is sunlight.

Mold growing an a clay having added xantham gum

Mold growing an a clay having added xantham gum

This slug is about 6 months old. It contains 0.75% gum. The gum also destroys the workability of the clay.