% Passing 200 Mesh Wet - P200

This test procedure was employed in the Foresight Ceramic Database and now is available for those having an account at Insight-Live.com. Accumulating test data using the variables defined in these procedures enables us to create tools that enable you to compare the physical properties of materials and recipes.

Notes

200 mesh is a critical line coarser than which materials intended for porcelains should not have particles, especially if they are speck producing.

Variables

VAL - Value (V)