LOI (100-1000C) - LOI

This test procedure was employed in the Foresight Ceramic Database and now is available for those having an account at Insight-Live.com. Accumulating test data using the variables defined in these procedures enables us to create tools that enable you to compare the physical properties of materials and recipes.

Notes

ASTM-20
The weight lost by a ceramic compound during firing. The loss is due to water and organic materials that turn to gases. It is assumed the sample has been boil dried. Some labs also do 25-100C LOI.

For a detailed test procedure, see the LDW test.

Variables

VAL - Value (V)

Enter LOI percent value

Out Bound Links

In Bound Links

  • (Articles) The Physics of Clay Bodies

    Learn to test your clay bodies and recording the results in an organized way and understanding the purpose of each test and how to relate its results to changes that need to be made in process and recipe.

  • (Tests) BLOI - Borate LOI

By Tony Hansen




Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved