•The secret to cool bodies and glazes is a lot of testing.
•The secret to know what to test is material and chemistry knowledge.
•The secret to learning from testing is documentation.
•The place to test, do the chemistry and document is an account at https://insight-live.com
•The place to get the knowledge is https://digitalfire.com

Sign-up at https://insight-live.com today.

Dry M.O.R. (50% Silica) - MOR5

This test procedure was employed in the Foresight Ceramic Database and now is available for those having an account at Insight-Live.com. Accumulating test data using the variables defined in these procedures enables us to create tools that enable you to compare the physical properties of materials and recipes.

Notes

This is expressed in default units of psi (lb/square inch) and the clay material being tested is mixed with 50% silica. This is done with ball clays since their high plasticity cracks test bars during drying.

Variables

VAL - Value (V)

Out Bound Links

In Bound Links

  • (Tests) MOR - Modulus of Rupture - Fired
  • (Articles) Binders for Ceramic Bodies

    An overview of the major types of organic and inorganic binders used in various different ceramic industries.


By Tony Hansen




Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved