Apparent Viscosity (cps) - AVSC

This test procedure was employed in the Foresight Ceramic Database and now is available for those having an account at Insight-Live.com. Accumulating test data using the variables defined in these procedures enables us to create tools that enable you to compare the physical properties of materials and recipes.

Notes

This figure is only relative if the materials being compared are mixed and diluted the same way. Specify solids content. Viscometers produce values in units known as a centipoise or cps.

Variables

VAL - Value (V)

Out Bound Links

  • (Glossary) Viscosity

    The term viscosity is used in ceramics most often to refer to the degree of fluidity of a slurry or suspension (the term 'shear' is often used when discussing viscosity, theoretically engineers understand viscosity in terms of layers particles or molecules that exhibit a friction that resists latera...

In Bound Links

  • (Tests) LQLM - Liquid Limit

By Tony Hansen




Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved