44MR | APPO | AVPS | AVSC | BDGC | BDLB | BLOI | BWIW | CCON | CDRY | CEC | CLWC | CMST | COLE | COVB | CSSS | DENS | DFAC | DFDM | DIEL | DNLP | DS | DSHR | DSRN | DSTR | DTMP | EBCT | EM20 | FRFU | FRRD | FRTG | FSHR | FSTR | GBMF | GEBR | GLAZ | GLFL | GLHD | GLLE | GSPT | GTTM | HDMI | HEGF | HMA | HMAN | HMOH | IFP | IWCT | L10M | L1M | L20M | L2M | L30M | L5 | L5M | LDW | LOI | LQLM | MDPS | MLRG | MOIP | MOR | MOR5 | MORD | OLAD | P200 | P325 | PBPO | PCE | pHPG | pHPW | PPD | PRSM | PSHP | RC | RHEO | SADR | SAMG | SCLE | SHAB | SIEV | SLBY | SOLU | SPHC | SSAB | SVWT | TGA | THCO | TNST | TREL | TRMN | TSFL | UPSD | WABS | WOPL | WRA | WSR | XREF

GSPT - Frit Softening Point Test

This almost always refers to frits which soften and melt over a fairly wide temperature range (most raw materials melt over a much narrower range). The softening point is the temperature at which the material begins to move, no longer exhibiting the properties of a solid. This property is normally quoted on frit data sheets (see ASTM C-24). Theoretically feldspars, for example, melt in a similar fashion, but manufacturers would never normally quote this property.

The softening point of a glass can be determined by examining the curve produced by a dilatometer. The line (representing increasing thermal expansion) climbs as temperature increases, going through the transition point (and accompanying steepening of the curve) to the softening point. This point is the peak of the curve, after that the line drops off vertically and melting proceeds.

Variables

VAL - Value (V)

Temperature (specify C or F)

Simple dilatometric curve produced by a dilatometer

Simple dilatometric curve produced by a dilatometer

Dialometric chart produced by a dilatometer. The curve represents the increase in thermal expansion that occurs as a glass is heated. Changes in the direction of the curve are interpreted as the transformation (or transition) temperature, set point and softening point (often quoted on frit data sheets). When the thermal expansion of a material is quoted as one number (on a data sheet), it is derived from this chart. Since the chart is almost never a straight line one can appreciate that the number is only an approximation of the thermal expansion profile of the material.

Links

Tests Pyrometric Cone Equivalent
Tests Co-efficient of Linear Expansion
Tests Glass Transition Temperature
Tests Heating Microscope Analysis for Frits
Tests I.F.P. (celsius)
Tests Glaze Melt Flow - Runway Test
Tests Frit Melting Range (C)
Glossary Frit
Frits are used in ceramic glazes for a wide range of reasons. They are man-made materials of controlled chemistry with many advantages or raw materials.
Glossary Melt Fluidity
Ceramic glazes melt and flow according to their chemistry and mineralogy. Observing and measuring the nature and amount of flow is important in understanding them.
Typecodes Material Tests
Test conducted primarily on materials use to make bodies or glazes.

By Tony Hansen


Tell Us How to Improve This Page

Or ask a question and we will alter this page to better answer it.

Email Address

Name

Subject

Message


Upload picture


Copyright 2008, 2015, 2017 https://digitalfire.com, All Rights Reserved