Temperature: 300C - 330C

Description:Copper carbonate basic decomposes
Type:State Change

Notes

Loses 28% weight as it decomposes to to the heat stable CuO

In Bound Links

  • (Materials) Copper Carbonate Basic - CuCO3.Cu(OH)2

    Cupric Carbonate, Copper (II) Carbonate, Azurite

  • (Temperatures) Decarbonation (200C-1000C)

    A wide range of carbonates are used in ceramics and each of these has its own thermal history. Within that is a range where they decompose to give off...

  • (Glossary) Carbon Burnout

    Ceramic bodies and glazes contain materials that release carbon as they decompose on heating. Clays, gums, plasticizers are examples. These can still be burning out at higher temperatures than most people realize (cone 04 or higher). That burning generates gases, if glazes are beginning to melt befo...


By Tony Hansen

•The secret to cool bodies and glazes is a lot of testing.
•The secret to know what to test is material and chemistry knowledge.
•The secret to learning from testing is documentation.
•The place to test, do the chemistry and document is an account at https://insight-live.com
•The place to get the knowledge is https://digitalfire.com

Sign-up at https://insight-live.com today.