Temperature: 900 - 1000

Description:Talc crystalline water vaporizes
Type:Eutectic

Notes

The crystalline (mechanical) water from talc evolves as a vapor. This is typically about 4% of the starting mass of the talc. Slower heating through this zone is appropriate for talc-containing single fire glazed bodies or those bisque fired below this range.

In Bound Links

  • (Materials) Talc - Mg3Si4O6 or 3MgO.4SiO2.H2O

    Magnesium Silicate, Steatite, French Chalk, Hydrated talc