Temperature: 850C

Description:Sodium Carbonate decomposes
Type:Decomposition

Notes

Decomposition occurs at melting point. CO2 and NaO are emitted.

In Bound Links

  • (Materials) Sodium Carbonate - Na2CO3 H2O or Na2O.CO2.H2O - The most common form of sodium carbonate

    Soda Ash, Sodium Caronate Monohydrate, Na2CO3

  • (Temperatures) Decarbonation (200C-1000C)

    A wide range of carbonates are used in ceramics and each of these has its own thermal history. Within that is a range where they decompose to give off...


By Tony Hansen

•The secret to cool bodies and glazes is a lot of testing.
•The secret to know what to test is material and chemistry knowledge.
•The secret to learning from testing is documentation.
•The place to test, do the chemistry and document is an account at https://insight-live.com
•The place to get the knowledge is https://digitalfire.com

Sign-up at https://insight-live.com today.



Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved