Temperature: 512C

Description:Hydrated lime decomposes (25% H2O)
Type:Decomposition

In Bound Links

  • (Materials) Hydrated Lime - CaO.H2O or Ca(OH)2

    Slaked Lime, Calcium Hydroxide, Calcium Hydrate


By Tony Hansen