Temperature: 500C - 600C

Description:Magnesite decomposition
Type:Decomposition

Notes

The process of removing the CO2 from magnesite to produce light magnesium carbonate is often called magnesite decarbonization. There is variation in the temperature ranges given for this phenomenon by different sources (e.g. some say 550-600C).