Temperature: 185C

Description:Copper hydroxide decomposes to CuO
Type:Decomposition

Notes

Loses about 18% weight as it decomposes to the heat stable CuO

In Bound Links

  • (Materials) Copper Hydroxide - Cu(OH)2

    Copper(II) hydroxide, Copper Hydrate, Cupric Hydroxide