Temperature: 1565C

Description:Iron oxide red decomposes
Type:Melting Point/Range

Notes

Fe2O3 decomposes to Fe3O4. Releases oxygen.

In Bound Links

  • (Materials) Iron Oxide Red - Fe2O3 - Synthetic Hematite

    Ferric Oxide, Red Iron Oxide, RIO, Iron(III) oxide, Fe2O3, Hematite