Temperature: 1082C

Description:Spodumene converts to beta phase
Type:State Change

Notes

Undergoes an irreversible phase transition to yield beta-spodumene. This is accompanied by an expansion of ~30% and a decrease in specific gravity from 3.2 to 2.4. After conversion to its beta form at spodumene enters a stage of great thermal stability.

In Bound Links

  • (Materials) Spodumene - Li2O.Al2O3.4SiO2 or LiAl(Si2O6)

By Tony Hansen

•The secret to cool bodies and glazes is a lot of testing.
•The secret to know what to test is material and chemistry knowledge.
•The secret to learning from testing is documentation.
•The place to test, do the chemistry and document is an account at https://insight-live.com
•The place to get the knowledge is https://digitalfire.com