Ravenscrag Cone 10 Oxidation Variegated White

Code: GR10-G
Modification Date: 2016-09-30 22:49:05
Member of Group: RVox10

MaterialAmountPercent
Ravenscrag Slip100.087.7%
Additions
Talc10.08.8%
Tin Oxide4.03.5%
 114.00  

Notes

Out Bound Links

XML to Paste Into Insight

<?xml version="1.0"?>
<recipes version="1.0" encoding="UTF-8">
<recipe name="Ravenscrag Cone 10 Oxidation Variegated White" id="96" date="2016-09-30" codenum="GR10-G">
<recipelines>
<recipeline material="Ravenscrag Slip" amount="100.000" unitabbr="kg" conversion="1.0000" added="0"/>
<recipeline material="Talc" amount="10.000" unitabbr="kg" conversion="1.0000" added="1"/>
<recipeline material="Tin Oxide" amount="4.000" unitabbr="kg" conversion="1.0000" added="1"/>
<url url="https://digitalfire.com/4sight/recipes/ravenscrag_cone_10_oxidation_variegated_white_96.html" descrip="Recipe page at digitalfire.com"/>
</recipelines>
<urls/>
</recipe>
</recipes>


By Tony Hansen




Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved