Cone 6 GA6-C variegated blue showing different thicknesses (4% rutile+ 20% frit 3134 in Alberta Slip)

The glaze is a dolomite matte fired to cone 10R. High fire reduction is among the best processes to exploit the variegating magic of rutile.