Al2O3 | B2O3 | BaO | C | CaO | CO2 | CoO | Cr2O3 | Cu2O | CuO | Fe2O3 | FeO | H2O | K2O | Li2O | LOI | MgO | MnO | MnO2 | Na2O | NiO | O | Organics | P2O5 | PbO | SiO2 | SnO2 | SO3 | SO4 | SrO | TiO2 | V2O5 | ZnO | ZrO | ZrO2

Others

Ag2O | AlF3 | As2O3 | As4O6 | Au2O3 | BaF2 | BeO | Bi2O3 | CaF2 | CdO | CeO2 | Cl | CO | CrO3 | Cs2O | CuCO3 | Dy2O3 | Er2O3 | Eu2O3 | F | Fr2O | Free SiO2 | Ga2O3 | GdO3 | GeO2 | HfO2 | HgO | Ho2O3 | In2O3 | IrO2 | KF | KNaO | La2O3 | Lu2O3 | Mn2O3 | MoO3 | N2O5 | NaF | Nb2O5 | Nd2O3 | Ni2O3 | OsO2 | Pa2O5 | PbF2 | PdO | PmO3 | PO4 | Pr2O3 | PrO2 | PtO2 | RaO | Rb2O | Re2O7 | RhO3 | RuO2 | Sb2O3 | Sb2O5 | Sc2O3 | Se | SeO2 | Sm2O3 | Ta2O5 | Tb2O3 | Tc2O7 | ThO2 | Tl2O | Tm2O3 | U3O8 | UO2 | WO3 | Y2O3 | Yb2O3

•The secret to cool bodies and glazes is a lot of testing.
•The secret to know what to test is material and chemistry knowledge.
•The secret to learning from testing is documentation.
•The place to test, do the chemistry and document is an account at https://insight-live.com
•The place to get the knowledge is https://digitalfire.com

Sign-up at https://insight-live.com today.

Se (Selenium)

FamilyOther
Weight111.200

Notes

-Semi-metallic element of the sulfur group. Its main value as a colorant depends on a reduction or mildly oxidizing atmosphere to maintain its metallic state.

-With cobalt it is a good decolorizer for glass because it produces a pink which is close to complementary of iron green (thus canceling it out).

-Used as a colorant in making rose and ruby glass.

-Used in some special purpose stains.

Mechanisms