Mineral: Sanidine

Notes

A potash feldspar mineral.

Out Bound Links

In Bound Links

  • (Materials - Parent mineral) Potash Feldspar - K2O.Al2O3.6SiO2

    K-Feldspar, Orthoclase, K Feldspar, Potassium Feldspar