Mineral: Plagioclase

Notes

A abundant sodium calcium feldspar mineral.
Na2O 9.5%, CaO 4.0%, Al2O3 22.5%, SiO2 68.7%

Out Bound Links

In Bound Links

  • (Materials) M74 Feldspar - Soda Feldspar
  • (Materials - Parent mineral) Andesine - Na2O.CaO.2Al2O3.8SiO2 - Plagioclase Feldspar
  • (Minerals - Related) Albite

    A plagioclase feldspar mineral.