Mineral: Oligoclase

Notes

A plagioclase feldspar.

In Bound Links

  • (Minerals - Related) Plagioclase

    A abundant sodium calcium feldspar mineral. Na2O 9.5%, CaO 4.0%, Al2O3 22.5%, SiO2 68.7%