Mineral: Na-Feldspar

Notes

Most common feldspars contain both sodium and potassium. The term Na-Feldspar designates one where the K2O/Na2O balance heavily favors Na2).

Stockpile of crude feldspar from MGK Minerals (India) deposit

Stockpile of crude feldspar from MGK Minerals (India) deposit

Closeup of feldspar deposit in the MGK Minerals quarry in India

Closeup of feldspar deposit in the MGK Minerals quarry in India

Out Bound Links

  • (Oxides) Na2O - Sodium Oxide, Soda

In Bound Links

  • (Materials) Clay 215

    Kil 215

  • (Materials) Clay 216

    Kil 216

  • (Materials) Clay 220

    Kil 220

  • (Materials) Clay 220

    Kil 220

  • (Materials) Clay 222

    Kil 222

  • (Materials) Clay 232

    Kil 232

  • (Materials) Clay 233

    Kil 233

  • (Materials) Feldspar 632

    Feldspat 632

  • (Materials) Feldspar 635

    Feldspat 635

  • (Materials) F7/SG Feldspar - Soda Feldspar
  • (Materials) F7/SE Feldspar - Soda Feldspar

    Feldspar Soda F7/SE

  • (Materials) F7 Feldspar - Soda Feldspar
  • (Materials) FM6 Feldspar - Sodium Potassium Feldspar
  • (Materials) KM71 Feldspar - Potash Feldspar
  • (Materials) FK45 Feldspar - Sodium Potassium Feldspar
  • (Materials) Aplite A/3
  • (Minerals - Related) Granite

    Granite is a plutonic rock is found throughout the continental crust, most commonly in mountainous areas (it is the most abundant type of rock). The matrix consists mainly of quartz grains (10-50%), p...

  • (Materials - Contained) Kaolin 233
  • (Minerals - Related) K-Feldspar

    Most common feldspars contain both sodium and potassium. The term K-Feldspar designates one where the K2O/Na2O balance heavily favors K2O.

  • (Minerals - Related) Feldspar

    An indispensable material in the ceramic industry. Most ceramic bodies employ feldspar as a flux to vitrify them at a lower temperature (the feldspar creates a glaze that glues the more refractory par...


By Tony Hansen




Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved