Zircosil

Zircopax Plus made by Endeka Ceramics

This is available in many particle sizes, each used for a specific industry or family of applications. Examples grade grades are S, D, 200, 200M, 300M, Ten, Five, One (the latter referring to micron sizes). The Five material is sold as "Zircopax Plus" in North America.


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Zircosil" descrip="Zircopax Plus made by Endeka Ceramics" searchkey="" loi="0.00" casnumber=""> </material>