Zinc Carbonate

Formula: ZnCO3
Alternate Names: Smithsonite, zinc spar

OxideAnalysisFormula
ZnO64.91%1.000
CO235.09
Oxide Weight81.40
Formula Weight125.40
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Zinc Carbonate" descrip="" searchkey="Smithsonite, zinc spar" loi="0.00" casnumber="3486-35-9"> <oxides> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="64.910" tolerance=""/> </oxides> <volatiles> <volatile symbol="CO2" name="Carbon Dioxide" percent="35.090" tolerance=""/> </volatiles> </material>