Window Glass

OxideAnalysisFormula
CaO8.54%0.323
MgO4.02%0.212
K2O0.10%0.002
Na2O13.55%0.463
Al2O30.50%0.010
B2O30.10%0.003
SiO272.79%2.568
Fe2O30.10%0.001
SO30.30
Oxide Weight211.41
Formula Weight212.05
If this formula is not unified correctly please contact us.

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Window Glass" descrip="" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="8.540" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="4.020" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.100" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="13.550" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="0.500" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="0.100" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="72.790" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.100" tolerance=""/> </oxides> <volatiles> <volatile symbol="SO3" name="Sulfur Trioxide" percent="0.300" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved