OxideAnalysisFormula
CaO0.10%0.005
TiO21.70%0.058
Al2O337.70%1.000
SiO245.80%2.062
Fe2O30.70%0.012
LOI13.20
Oxide Weight232.68
Formula Weight268.06
If this formula is not unified correctly please contact us.
PCE - Pyrometric Cone Equivalent 34

Wilco UPF is finer grained kaolin and can be employed in a ceramic formulation where higher permeability type kaolin is not required. It has excellent suspension qualities and lends good film strength to ceramic engobes and glazes of all temperature ranges. Wilco UPF also meets the requirements of filler applications where a dry ground processed kaolin can be employed.

This is not suitable for use in making plastic bodies that depend primarily on it for the plasticity. Thus it cannot be used in recipes as a substitute for #6 Tile kaolin, for example.


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Wilco-UPF Kaolin" descrip="" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.100" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="1.700" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="37.700" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="45.800" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.700" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="13.200" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved