OxideAnalysisFormula
CaO5.08%0.385
MgO2.43%0.256
K2O1.38%0.062
Na2O4.33%0.297
TiO20.59%0.031
Al2O317.48%0.728
SiO262.51%4.420
Fe2O35.35%0.142
MnO0.07%0.004
LOI0.77
Oxide Weight421.61
Formula Weight424.88
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Volcanic Ash" descrip="From Ron Roy's MDT" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="5.080" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="2.430" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="1.380" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="4.330" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.590" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="17.480" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="62.510" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="5.350" tolerance=""/> <oxide symbol="MnO" name="Manganous Oxide" status="" percent="0.070" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="0.770" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved