vol660cer

MICRON-SIZE SODIUM HECTORITE

OxideAnalysisFormula
CaO1.19%0.165
MgO3.01%0.582
K2O0.31%0.026
Na2O1.81%0.227
TiO20.15%0.015
Al2O319.40%1.481
SiO263.80%8.269
Fe2O34.16%0.203
LOI6.10
Oxide Weight730.84
Formula Weight778.32
If this formula is not unified correctly please contact us.

A grit-free, high purity, gray sodium bentonite of micron-sized particles used as a general purpose suspending agent and binder.

Specific Gravity: 2.5
pH (5% dispersion): 8.5-10.0
C.E.C. (meq/100g): 104
Dry Brightness (Green Filter): 67
Color: Gray
% Moisture Content: 12% Max.
Brookfield Viscosity (60 rpm @ 5% solids): 353cps


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="vol660cer" descrip="MICRON-SIZE SODIUM HECTORITE" searchkey="" loi="6.10" casnumber="12173-47-6"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="1.190" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="3.010" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.310" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="1.810" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.150" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="19.400" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="63.800" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="4.160" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="6.100" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved