vol446cer

SODIUM BENTONITE GRANULES

OxideAnalysisFormula
CaO1.06%0.093
MgO2.67%0.326
K2O0.36%0.019
Na2O7.08%0.562
TiO20.13%0.008
Al2O316.60%0.801
SiO251.70%4.234
Fe2O33.31%0.102
LOI17.10
Oxide Weight408.10
Formula Weight492.27
If this formula is not unified correctly please contact us.

Sodium bentonite granules, agglomerated from 325 mesh bentonite. It is fast dispersing and is used as a suspending agent in glazes and a binder for pencil lead.

Specific Gravity: 2.5
pH (5% dispersion): 8.5-10.5
C.E.C. (meq/100g): 82
Dry Brightness (Green Filter): 65
Color: Yellow
% Moisture Content: 12% Max.
Brookfield Viscosity (60 rpm @ 5% solids): 532cps


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="vol446cer" descrip="SODIUM BENTONITE GRANULES" searchkey="" loi="17.10" casnumber="52623-66-2"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="1.060" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="2.670" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.360" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="7.080" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.130" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="16.600" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="51.700" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="3.310" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="17.100" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved