OxideAnalysisFormula
CaO1.89%0.215
MgO3.44%0.544
K2O1.06%0.072
Na2O1.65%0.170
TiO21.47%0.117
Al2O313.00%0.812
SiO270.10%7.433
Fe2O31.45%0.058
LOI5.90
Oxide Weight599.43
Formula Weight637.02
If this formula is not unified correctly please contact us.

A highly purified, white, sodium bentonite supplied as a free-flowing powder. Used when high purity and high whiteness are important in suspending glazes.

Specific Gravity: 2.5
pH (5% dispersion): 9.0-10.0
C.E.C. (meq/100g): 70
Dry Brightness (Green Filter): 87
Color: White
% Moisture Content: 10% Max.
Brookfield Viscosity (60 rpm @ 5% solids): 1098cps


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="vol364cer" descrip="White Sodium Bentonite" searchkey="" loi="5.90" casnumber="52623-66-2"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="1.890" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="3.440" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="1.060" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="1.650" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="1.470" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="13.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="70.100" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="1.450" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="5.900" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved