FINE WHITE CALCIUM HECTORITE

OxideAnalysisFormula
CaO4.04%0.125
Li2O1.50%0.087
MgO17.90%0.768
K2O0.33%0.006
Na2O0.50%0.014
TiO20.20%0.004
Al2O34.21%0.071
SiO244.10%1.269
Fe2O31.36%0.015
LOI25.80
Oxide Weight128.25
Formula Weight172.84
If this formula is not unified correctly please contact us.

Finely ground, white, calcium hectorite clay. Used as a binder in extruded tile to increase green strength with minimum increases in viscosity.

Specific Gravity: 2.5
pH (5% dispersion): 8.5-9.5
C.E.C. (meq/100g): 104
Dry Brightness (Green Filter): 71
Color: White
% Moisture Content: 10% Max.
Brookfield Viscosity (60 rpm @ 5% solids): 24cps


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="vol355cer" descrip="FINE WHITE CALCIUM HECTORITE" searchkey="" loi="25.80" casnumber="12173-47-6"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="4.040" tolerance=""/> <oxide symbol="Li2O" name="Lithium Oxide, Lithia" status="" percent="1.500" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="17.900" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.330" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.500" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.200" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="4.210" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="44.100" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="1.360" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="25.800" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved