PURIFIED HECTORITE

OxideAnalysisFormula
CaO3.53%0.106
MgO18.10%0.760
K2O0.40%0.007
Na2O4.65%0.127
TiO20.17%0.004
Al2O33.59%0.060
SiO250.70%1.427
Fe2O30.94%0.010
LOI17.80
Oxide Weight138.81
Formula Weight168.87
If this formula is not unified correctly please contact us.

An economical blend of beneficiated purified hectorite. Used to promote optimum surface hardening of unfiring ceramic glazes.

Specific Gravity: 2.5
pH (5% dispersion): 9.5-10.5
C.E.C. (meq/100g): 120
Dry Brightness (Green Filter): 75
Color: White
% Moisture Content: 10% Max.
Brookfield Viscosity (60 rpm @ 5% solids): 12,020 cps


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="vol334cer" descrip="PURIFIED HECTORITE" searchkey="" loi="17.80" casnumber="12173-47-6"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="3.530" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="18.100" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.400" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="4.650" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.170" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="3.590" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="50.700" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.940" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="17.800" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved