vol331cer

WHITE FINE SODIUM BENTONITE

OxideAnalysisFormula
CaO1.25%0.136
MgO3.87%0.585
K2O1.26%0.082
Na2O2.01%0.198
TiO20.12%0.009
Al2O313.40%0.801
SiO258.70%5.952
Fe2O32.21%0.084
LOI17.20
Oxide Weight504.67
Formula Weight609.51
If this formula is not unified correctly please contact us.

A finely ground, white, sodium bentonite, supplied as a free flowing white powder. Used as a suspending agent in glazes when white color is important.

Specific Gravity: 2.5
pH (5% dispersion): 9.0-10.0
C.E.C. (meq/100g): 100
Dry Brightness (Green Filter): 85
Color: White
% Moisture Content: 10% Max.
Brookfield Viscosity (60 rpm @ 5% solids): 146cps


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="vol331cer" descrip="WHITE FINE SODIUM BENTONITE" searchkey="" loi="17.20" casnumber="52623-66-2"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="1.250" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="3.870" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="1.260" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="2.010" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.120" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="13.400" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="58.700" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="2.210" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="17.200" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved